Defects and solutions that are easy to occur in veneer drying

(1) Veneer deformation and cracking

Reason: There is a difference between the early and late wood in the veneer. The wood itself has knots and other unevenness of the veneer structure, which causes the veneer to have a difference in shrinkage during the drying process, thereby causing deformation and cracking of the veneer.

In addition, during the drying process of the veneer, the moisture at the edge of the veneer is faster than that in the middle, and the shrinkage deformation at the edge of the veneer is limited by the middle portion, so the edge is prone to wave shape and sometimes even crack.

Solution: 1. When the single or fast veneer is fed into the dryer longitudinally, the front and rear plate edges should overlap by 1-2 cm, so that the evaporation speed of the single edge can be reduced, and the central portion is close to the same. Prevent deformation and cracking.

2. When the strip is continuously dried on one side, water can be sprayed on the width of 6 mm on both sides of the single side to increase the moisture content of the edge of the veneer to delay the drying speed of the edge and reduce wave deformation and cracking.

3. When the strip-shaped veneer is continuously dried, a reinforcing tape or a glue line may be attached on both sides of the wet veneer to increase the strength in the direction of the horizontal stripes and prevent the end plate from being cracked.

(2) Uneven water content of veneers

When the tree species, thickness and storage time of the veneer are the same, the final water content of the veneer is inconsistent after drying, which is often caused by the difference in the initial water content and the drying speed of the veneer and the sapwood. Differences in temperature, humidity, and wind speed at different locations and in different layers in the dryer may also cause unevenness in the final moisture content of the veneer after drying.

The solution method is as follows: 1. The tree species with different water content of the heart and the sapwood (such as pine), the spin-cut veneers are dried separately according to the heart and the sapwood.

2. The microwave-convection heating composite dryer uses the selective heating characteristics of the microwave to make the moisture content of the veneer even after drying.

5. Dry Weave Sanitary Napkins

 

Product description of dry weave Sanitary Napkins

1. Slim 5mm, 240mm long.

2. Super dry net , anti-rewet.

3. Super absorbent & keep dry and fresh at any moment.

4. NO stains left on the cover after absorption.

5. Perfect body fit, firmly being kept on the panty without any side leakage.

6. Individually wrapped.

Safe Sanitary Pads 

 

FAQ:

What is your Min. order quality?

A: One twenty-foot container, small quality available if has stock

 

Your supply ability?

A: 5,000,000 piece/pieces per week sanitary napkins in bulk

 

What is your neareast port?

A: Shenzhen

 

What is the payment terms you accepted?

A L/C, T/T, Western union, MoneyGram

Dry Weave Sanitary Napkins

Dry Weave Sanitary Napkins,Sanitary Towel,Sanitary Napkins,Sanitary Products

Glory Power Hygiene Products Ltd. , https://www.hygienenapkin.com